• This community needs YOUR help today. We rely 100% on Supporting Memberships to fund our efforts. With the ever increasing fees of everything, we need help. We need more Supporting Members, today. Please invest back into this community. I will ship a few decals too in addition to all the account perks you get.



    Sign up here: https://www.muzzleloadingforum.com/account/upgrades
  • Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Rust Blueing

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
It works exceptionally well.

DO follow their instructions. Rust blue takes a little longer than browning for sure, but it is absolutely worth going that route.

The end product is excellent.

If you end up going with this product "for sure", do a search in some past posts here.

There are a number of "different" methods to (boil the barrel), when you get to that stage.

All of them seem to work and produce exactly the same results.

Rust blue isn't rocket science by any means - just a "kinda slow" step by step to get you to the finished product.
 
That's what I used on this CVA 12 guage double.

The water boil was done with a turkey roasting pan and the barrel wouldn't fit into it so I used a glass measuring cup to dip and pour the water over the center of the barrel. :hmm:

 
I did the bath method. Used a PCV pipe "trough" and poured the scalding water in. I did go cheap and used two pieces glued together (had them laying around in the garage) but it worked.

Here's the link Link
 