This community needs YOUR help today. We rely 100% on Supporting Memberships to fund our efforts. With the ever increasing fees of everything, we need help. We need more Supporting Members, today. Please invest back into this community. I will ship a few decals too in addition to all the account perks you get.
Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.
We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.
Good luck and be assured that pouring nose caps is not that hard, but good preparation is the key, along with a good continued pour, and leaving enough metal towards the front for shaping. Get the metal temperature right, and Bob's your uncle! -P.S.- The first pour or two might look like something Quasimodo blew out of his nose, but that's OK, we live to learn.
Here's some photos of the process I use to pour a nose cap. I use tin with 5% antimony added. That's just 95/5 solder I pickup at yard sales for cheap. The cap needs final polishing. It seems to keep from oxidizing like some metals do.
Great job, thanks for the response. I did one once on a Sharon Hawken using pewter. But that was 35 years ago. Not so sure I want to tackle it again. I would if I thought it would turn out as good as yours.
Maybe, yours sure looks great.