• This community needs YOUR help today. We rely 100% on Supporting Memberships to fund our efforts. With the ever increasing fees of everything, we need help. We need more Supporting Members, today. Please invest back into this community. I will ship a few decals too in addition to all the account perks you get.



    Sign up here: https://www.muzzleloadingforum.com/account/upgrades
  • Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Patching material

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
I have shot at the Texas State ML match a number of times. The "Texas Patch", which is sail cloth coated on one side with Blue Teflon. The patch is lubed on the ball side with a small amount of water. These patches are very remarkable for improved accuracy. You must wipe the bore each time before loading. I buy this patch material from fellow in Wichita Falls.
 
Redwing,
Sure enough...stay here long enough, and you'll learn something new. I've used dry teflon patch material off and on over the years, but never heard anyone discuss wetting it.
What do you reckon wetting the ball side does..??
Have you ever fired side-by-side comparison groups...dry vs. damp..??
Thanks for the idea :hatsoff: ...now I have a whole other variable to mess with...!!! :doh:
 