• This community needs YOUR help today. We rely 100% on Supporting Memberships to fund our efforts. With the ever increasing fees of everything, we need help. We need more Supporting Members, today. Please invest back into this community. I will ship a few decals too in addition to all the account perks you get.



    Sign up here: https://www.muzzleloadingforum.com/account/upgrades
  • Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Tang thickness question

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Crow#21957

50 Cal.
Joined
Dec 26, 2022
Messages
1,494
Reaction score
915
Location
Mooreland Indiana
I've got a long tang about 6 in. On this build.
The tang is pretty thick. Would you thin the tang or just remove enough wood to get it in?±
I hate removing that much wood. Second do you heat a tang to make it was to bend or just bent it cold? Almost 1/4 in. Thick.
Ok
 
I've got a long tang about 6 in. On this build.
The tang is pretty thick. Would you thin the tang or just remove enough wood to get it in?±
I hate removing that much wood. Second do you heat a tang to make it was to bend or just bent it cold? Almost 1/4 in. Thick.
Ok
I can't answer with respect to historically correct, just what I would do. A tang 3/16" thick is adiquate even if you were to shave a little of that to conform to the stock curvature. Heating to me is relative to the sharpness of the bend. Most tangs would not require heat. This is my opinion.