• This community needs YOUR help today. We rely 100% on Supporting Memberships to fund our efforts. With the ever increasing fees of everything, we need help. We need more Supporting Members, today. Please invest back into this community. I will ship a few decals too in addition to all the account perks you get.



    Sign up here: https://www.muzzleloadingforum.com/account/upgrades
  • Friends, our 2nd Amendment rights are always under attack and the NRA has been a constant for decades in helping fight that fight.

    We have partnered with the NRA to offer you a discount on membership and Muzzleloading Forum gets a small percentage too of each membership, so you are supporting both the NRA and us.

    Use this link to sign up please; https://membership.nra.org/recruiters/join/XR045103

Smoothbore load testing

Muzzleloading Forum

Help Support Muzzleloading Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Zonie said:
Even JB Weld doesn't like heat.

It can take a lot more heat than most epoxy's but if the area is heated up to temperatures around 400°F it will lose its strength and release whatever it's holding.

These temperatures are similar to those used for soft soldering and won't harm or change steel.
Sounds like a better plan than mine! :grin:
 
Thanks for posting your results.
Was just banging off the back porch with the fifty smoothie and cogitatin' on small ball. I'm thinking .465 ball is next up for tests.
 
I needed to put a new front sight on my fowler. My soldering skills are seriously lacking, so I used JB weld. held tight as can be and when it was time to take it off and solder it properly it came right off with a torch
 